Defects in forgings caused by defects in raw materials
1. Surface crack
2. The folding
3. The scar
4. Layered fracture
5. Bright line (bright area)
6. Non-metallic inclusion
7.Carbide segregation
8. Aluminum oxide film
9. The white dots
10.The coarse grain ring